Experimental and Data Analysis Workflow for Soft Matter Nanoindentation

5.5K views

Cited by 19

13:04 min

January 18th, 2022

10.3791/63401-v

January 18th, 2022

5.5K views
 ,  ,  ,  ,  , 

The protocol presents a complete workflow for soft material nanoindentation experiments, including hydrogels and cells. First, the experimental steps to acquire force spectroscopy data are detailed; then, the analysis of such data is detailed through a newly developed open-source Python software, which is free to download from GitHub.

Explore More Videos

Nanoindentation Workflow

Chapters in this video

0:05

Introduction

0:43

Probe Calibration

3:38

Measuring the Young s Modulus of Soft Materials

5:30

Data Analysis

6:33

Formal Data Analysis

10:08

Results: Acquiring Nanoindentation Data on Hydrogels and Cells

12:26

Conclusion

Related Videos