新鲜混凝土中的泌水发生在混合物中的水上升到表面时。这是因为混合物的固体成分在沉降时无法保留所有水,导致水在顶部聚集而分离。可以通过评估总沉降或注意每单位高度的混凝土高度下降来衡量泌水的严重程度。
泌水会导致混凝土结构出现多种问题。有时,上升的水会被困在大型骨料颗粒或钢筋下方,从而在混凝土内形成空隙。…
如果混凝土拌合物中的水上升到新浇筑混凝土的表面,则称为泌水。其原因是拌合物中的固体在沉降过程中无法保持全部水分。
通过测量混凝土单位高度的总沉降量或高度减少量,可量化出血程度。
有时,上升的水分会被困在粗骨料颗粒或钢筋下方,形成空隙。
如果这些孔隙呈对齐分布,可能会使混凝土在水平方向上更具渗透性。
如果上升的水携带大量细小的水泥颗粒,会在板面形成一层弱而多孔的物质,称为浮浆,导致表面出现粉状质地,从而形成脆弱层面,影响与后续混凝土层的粘结性能。
通过刷洗和冲洗去除浮浆至关重要,因为浮浆若包裹住气泡或泌水,会形成 blister(水泡)。
细度更高的水泥、更高的碱含量或三氧化二铝含量,或添加氯化钙均可减少泌水,尽管这些方法可能存在某些缺点。
此外,引气能有效减少泌水,从而在混凝土浇筑后立即实现更快的收面处理。
View the full transcript and gain access to JoVE Core videos
Q1: What causes bleeding in fresh concrete?
Bleeding occurs when water from the concrete mix rises to the surface because the mix's solid components fail to retain all water as they settle. This separation causes water to collect at the top of the newly laid concrete. The extent of bleeding can be measured by assessing total settlement or the decrease in height per unit height of concrete.
Q2: How does bleeding affect concrete permeability and surface quality?
Rising water can become trapped beneath large aggregate particles or reinforcement, creating voids that increase horizontal permeability if they align. Additionally, when ascending water carries fine cement particles to the surface, it forms laitance—a weak, porous layer with a dusty texture. This layer creates a fragile plane that compromises adhesion with subsequent concrete layers and can form blisters if it traps air bubbles.
Q3: What is laitance and why must it be removed from concrete?
Laitance is a weak, porous layer that forms on the concrete surface when rising water transports fine cement particles upward. Removing laitance by brushing and rinsing is crucial because it creates a fragile plane that weakens adhesion between concrete layers and can trap air bubbles or bleeding water, forming blisters that compromise structural integrity.
Q4: How can finer cement and chemical additives reduce bleeding?
Bleeding decreases with finer cement, which improves water retention in the mix. Adding substances with higher alkali or tricalcium aluminate content also reduces bleeding. Calcium chloride is another effective additive, despite potential drawbacks. These modifications help stabilize the mix and minimize water separation at the surface.
Q5: What role does air entrainment play in controlling bleeding?
Air entrainment effectively reduces bleeding in concrete by improving the mix's ability to retain water and stabilize the structure. By incorporating air bubbles into the concrete, this technique enables a quicker and more efficient finishing process immediately after casting, while simultaneously minimizing water separation and surface defects.
Q6: How is bleeding severity measured in fresh concrete?
The severity of bleeding is quantifiable by measuring the total settlement or by calculating the decrease in height per unit height of concrete. These measurements provide a numerical assessment of how much water has risen to the surface, helping engineers evaluate the quality of the concrete mix and determine if mitigation strategies are needed.
Q7: How does bleeding relate to factors affecting workability?
Bleeding is influenced by factors affecting workability, including cement fineness, water content, and mix composition. Understanding these factors affecting workability helps engineers design concrete mixes that minimize bleeding while maintaining adequate workability for proper placement and consolidation during construction operations.