Atomic Force Microscopy Cantilever-Based Nanoindentation: Mechanical Property Measurements at the Nanoscale in Air and Fluid

4.1K views

Cited by 11

08:58 min

December 2nd, 2022

10.3791/64497-v

December 2nd, 2022

4.1K views
 ,  ,  ,  ,  ,  ,  ,  ,  ,  ,  , 

Quantifying the contact area and force applied by an atomic force microscope (AFM) probe tip to a sample surface enables nanoscale mechanical property determination. Best practices to implement AFM cantilever-based nanoindentation in air or fluid on soft and hard samples to measure elastic modulus or other nanomechanical properties are discussed.

Explore More Videos

Nanoindentation Technique

Chapters in this video

0:05

Introduction

0:58

Sample Preparation and Instrument Setup

2:05

Probe Calibration

4:15

Collecting Force-Displacement (F-D) Data

5:58

F-D Curve Analysis

6:44

Results: Recent Advances in Atomic Force Microscopy for Surface Property Studies

8:07

Conclusion

Related Videos