Atomic Layer Deposition

Atomic Layer Deposition (ALD) is a thin-film fabrication method that builds materials one atomic-scale layer at a time, enabling precise thickness control and highly conformal coatings on complex surfaces. In each cycle, alternating gaseous precursors react with surface sites in self-limiting reactions, with purge steps separating exposures to prevent unwanted gas-phase reactions. This controlled process supports dielectric, conductive, and protective films for semiconductor devices, energy systems, optics, and nanostructured components, where uniform coverage and nanoscale interfaces influence performance, reliability, and device integration.

Atomic Layer Deposition - Related Videos

Research

JoVE Journal - Engineering

Making Record-efficiency SnS Solar Cells by Thermal Evaporation and Atomic Layer Deposition

0 Views •

Cited by 31 •

2015

Tin sulfide (SnS) is a candidate material for Earth-abundant, non-toxic solar cells. Here, we demonstrate the fabrication procedure of the SnS solar cells employing atomic layer deposition, which yields 4.36% certified power conversion efficiency, and thermal evaporation which yields 3.88%.

Epitaxial Growth of Perovskite Strontium Titanate on Germanium via Atomic Layer Deposition

0 Views •

Cited by 3 •

2016

This work details the procedures for the growth and characterization of crystalline SrTiO3 directly on germanium substrates by atomic layer deposition. The procedure illustrates the ability of an all-chemical growth method to integrate oxides monolithically onto semiconductors for metal-oxide semiconductor devices.

Layer-by-layer Collagen Deposition in Microfluidic Devices for Microtissue Stabilization

0 Views •

Cited by 7 •

2015

The creation of functional microtissues within microfluidic devices requires the stabilization of cell phenotypes by adapting traditional cell culture techniques to the limited spatial dimensions in microdevices. Modification of collagen allows the layer-by-layer deposition of ultrathin collagen assemblies that can stabilize primary cells, such as hepatocytes, as microfluidic tissue models.

Research

JoVE Journal - Engineering
Free Sample

Atomic Layer Deposition of Vanadium Dioxide and a Temperature-dependent Optical Model

0 Views •

Cited by 15 •

2018

Thin films (100-1000 Å) of vanadium dioxide (VO2) were created by atomic-layer deposition (ALD) on sapphire substrates. Following this, the optical properties were characterized through the metal-insulator transition of VO2. From the measured optical properties, a model was created to describe the tunable refractive index of VO2.

Research

JoVE Journal - Chemistry
Free Sample

Improved Heterojunction Quality in Cu2O-based Solar Cells Through the Optimization of Atmospheric Pressure Spatial Atomic Layer Deposited
Zn1-xMgxO

0 Views •

Cited by 5 •

2016

Here we present a protocol for synthesizing Zn1-xMgxO/Cu2O heterojunctions in open-air at low temperature via atmospheric pressure spatial atomic layer deposition (AP-SALD) of Zn1-xMgxO on cuprous oxide. Such high quality conformal metal oxides can be grown on a variety of substrates including plastics by this cheap and scalable method.

View All Results