Ultrasound Velocity Measurement in a Liquid Metal Electrode

11.4K views

Cited by 14

08:41 min

August 5th, 2015

10.3791/52622-v

August 5th, 2015

11.4K views

Ultrasound velocimetry is used to study mixing by fluid flow in liquid metal electrodes. The focus of this manuscript is to illustrate the methods used for making precise, spatially-resolved ultrasound measurements while limiting oxidation and controlling and monitoring temperature, applied current, and the heater power being supplied.

Explore More Videos

Sound Speed Measurement

Chapters in this video

0:05

Title

1:25

System Setup, Assembly and Sound Speed Measurement

3:32

Ultrasound Velocity Measurement

6:10

Results: Ultrasound Velocity Measurements of ePbBi

7:53

Conclusion